Abstract
The electrochromic characteristics of tungsten oxide films are largely affected by deposition conditions, such as substrate temperature and gas flow rate and also post-annealing. We have considered gas flow rate and temperature as important factors having an effect on an electrical, optical phenomenon and structural variation of $WO_3$ . The tungsten oxide films were deposited onto ITO(20$\Omega\box$, 1000$\AA$) using rf magnetron sputtering method. In particular, the films deposited at room temperature were annealed at various temperatures in air. All specimens had crystal structure except one being deposited at room temperature with nearly amorphous-like structure. The specimen deposited at $100^{\circ}C$ had a structure in which the increase in deposition temperature. The specimen deposited at $100^{\circ}C$ had a structure in which the cations$(Li^+)$ are easily movable because of void boundaries induced by regularly arrayed large grains. The specimen deposited at $300^{\circ}C$ had a dense structure with small grains but it exhibited the large mobility and charge density in $WO_3$ because of distinct grain boundaries.