Material Integrity Assessment for a Ni Electrodeposit inside a Tube

  • Kim, Dong-Jin (Division of Nuclear Material Technology Developments, Korea Atomic Energy Research Institute(KAERI)) ;
  • Kim, Myong Jin (Division of Nuclear Material Technology Developments, Korea Atomic Energy Research Institute(KAERI)) ;
  • Kim, Joung Soo (Division of Nuclear Material Technology Developments, Korea Atomic Energy Research Institute(KAERI)) ;
  • Kim, Hong Pyo (Division of Nuclear Material Technology Developments, Korea Atomic Energy Research Institute(KAERI))
  • Published : 2007.10.31

Abstract

Due to the occasional occurrence of a localizedcorrosion such as a SCC and pitting in steam generator tubing(Alloy 600), leading to a significant economical loss, an effective repair technology is needed. For a successful electrodeposition inside a tube, many processes should be developed. Among these processes, an anode to be installed inside a tube, a degreasing condition to remove any dirt and grease, an activation condition for a surface oxide elimination, a strike layer forming condition which needs to be adhered tightly between an electroforming layer and a parent tube and a condition for an electroforming layer should be established. Through a combination of these various process condition parameters, the desired material properties can be acquired. Among these process parameters, various material properties including a mechanical property and its variation along with the height of the electrodeposit inside a tube as well as its thermal stability and SCC resistance should be assessed for an application in a plant. This work deals with the material properties of the Ni electrodeposits formed inside a tube by using the anode developed in this study such as the current efficiency, hardness, tensile property, thermal stability and SCC behavior of the electrodeposit in a 40wt% NaOH solution at $315^{\circ}C$. It was found that a variation of the material properties within the entire length of the electrodeposit was quite acceptable and the Ni electrodeposit showed an excellent SCC resistance.

Keywords

References

  1. P. E. MacDonald, V. N. Shah, L. W. Ward and P. G. Ellison, NUREG/CR 6365, INEL 95/0383 , p. 36, (1996)
  2. F. Gonzalez, A. M. Brennenstuhl, G. Palumbo, U. Erb and P.C. Lichtenberger, Materials Science Forum, 225-227, 831 (1996)
  3. M.G. Fontana, Corrosion Engineering, Vol. 3, B & Jo Enterprise, Singapore, 1986
  4. J. E. Williams and C. Davison, J. Electrochem. Soc., 137, 3260 (1990)
  5. M. Schlesinger and M. Paunovic, Modern Electroplating, 4th ed., p. 555, John Wiley & Sons, lnc., (2000)
  6. H. Zhang and S.M. Park, J. Appl. Electrochem ., 24, 1182 (1994)
  7. D.-J. Kim, Y. M. Roh, M. H. Seo and J. S. Kim, Surf. and Coat. Tech., 192, 88 (2005)
  8. D.-J. Kim, H. P. Kim, J. S. Kim, K. W. Urm and S. H. Lee, Solid State Phenomena, 119, 87 (2007)
  9. D.-J. Kim, M. J. Kim, J. S. Kim and H. P. Kim, submitted to Materials and Corrosion (2007)